PEEK injection molding, Lu Rui plastics industry to answer your questions:

There are air holes in PEEK injection molding for the following reasons:

1, insufficient drying of raw materials.

2. The injection pressure is not enough and the firing rate is too fast.

The gate is too small

4. Exhaust slot is not set.

5, stored too fast, there are bubbles in the process of plasticization.

In view of the above situation, we can make corresponding adjustments.