1, making dies, convex and concave dies.
2. Cut the carbon fiber prepreg into a shape larger than a circular ring, and the allowance coefficient is 5%.
3. Brush the mold release agent, put the cut carbon fiber prepreg ring into the female mold, flatten it and put it into the male mold.
4. Put in a hot press, heat and pressurize for 30 minutes and then cure.
This is a standard process and easy to operate. It can be cured by heating without a mold.