Ordinary 32.5 cement: 1.00
Sand (fine aggregate):
1.38
Stones (coarse aggregate): 3:.83:
Water (tap water): 0.58
The strength grade of constructional column concrete is generally C20, and C25 can be used for buildings with high requirements.